HT 7000 | One part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HT7010 | One part Hybrid Gap Filler

Main features

  • Dark Red
  • 7 Thermal Conductivity
  • Horizontal mounting

Product Description

HT7000 silicone based one-part Gap Filler provides a thermal conductivity of 7.0 W/m·K along with high conformability and high compressibility. It is formulated to deliver high dispense rates for improved productivity, long-term reliability performance and to be easily reworkable.

HT7000 is designed to minimize thermal resistance at interfaces, maintain excellent performance through reliability testing, and provide scalable applications at a competitive cost.  Additionally it performs great in oil,crack and slump testing and it exhibits no pump out and cracking risk.

 

Product Family

233539

300cc Al cartridge
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Cartridge
Net weight 1.04 kg
Gross weight 1.14 kg
Dimensions 22 x 4.7 x 4.7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Dark Red
Dispense rate
Dispense rate is the amount of material that can be dispense from a nozzle in a specified time period. Please consult the TDS for the exact measurement conditions.
14 g/min
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.45
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
7 W/m.K
Thermal Impedance
1.41 °C·cm²/W

Additional Information

What properties of HT7000 will be greatly impacted when use beyond the expiration date?

Using HT7000 beyond its expiration date can significantly impact its properties. Thermal hybrid gels, such as HT7000, tend to be more sensitive to aging compared to phase change materials.
While oil separation is a common concern, it is not the sole issue that may arise with expired thermal gels.
Specifically, for HT7000, a noticeable drop in flow rate has been observed, which can negatively affect the customer's production line.

If a customer intends to use expired material, it is strongly recommended to conduct thorough quality testing to assess its suitability before proceeding.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers