ABLESTIK 8361J

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 8361J

Main features

  • Excellent dispensability
  • 1mil Spacers
  • Minimal voiding

Product Description

LOCTITE ABLESTIK 8361J die attach epoxy adhesive is designed for high reliability packaging applications. This electrically conductive epoxy offers high purity and minimal resin bleed, together with a low amount of condensable volatiles. 

LOCTITE ABLESTIK 8361J exhibits minimal tailing and stringing, along with minimal voiding. It stands out for its excellent strength retention after temperature and humidity exposure and its moderate stress absorption properties. Please note that this product contains 1mil silver spacers for a more controlled bondline.

Cure Schedule

  • 1 hour @ 175°C
  • 30 minute ramp to 115°C + 30 minutes @ 175°C
Product Family

213514

5 cc - Syringe
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Syringe
Net weight 17 g
Gross weight 21.95 g
Dimensions 2.8 x 1.4 x 7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
40 °C
Weight Loss @ 300°C
0.3 %
Chemical Properties
Moisture absorption
0.65 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
4.5
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
9,000 mPa.s

Leading Brands Trust in Our Products and Services